Effect of low vacuum medium temperature drying on reduction of residual stress and correction of warp of Japanese cedar timber

Zhuoting Jiang, Hiroyuki Yamamoto, Masato Yoshida, Motoo Dohi, Kento Tanaka, Kana Yamashita, Ken Watanabe

3 lipca 2024 · European Journal of Wood and Wood Products

Streszczenie

Brak zatwierdzonego streszczenia. Przeczytaj abstrakt poniżej lub otwórz oryginalną publikację.

Abstrakt

Cryptomeria japonica (Japanese cedar) in Japan plantations are aging, and the main supply of timber in the market is shifting from small- and medium-diameter to large-diameter logs. The effective utilization of these logs has become an important issue in the timber industry. When producing timber-without-pith from large-diameter logs, an unavoidable warp occurs because of the release of residual stress within the logs. Utilizing high-temperature drying with a load on these timbers has achieved significant drying effects, and the residual stress-induced warp was corrected. However, high-temperature drying has drawbacks, such as high energy consumption and the potential for thermal degradation. We applied low-vacuum-medium-temperature drying (LVMT-drying, 10 days, 40 kPa, 80/55 °C (DB/WB)—90/65 °C (DB/WB)) with load (650 kgf/m2) to the stacked timber sawn from large-diameter logs to address these questions. When LVMT-drying was successful, residual stresses in timber-with-pith were reduced to nearly zero, and warps in timber-without-pith were reduced to less than 8 mm, i.e., below the Japan Agriculture Standard "Level 1" for 4000 mm timber, and the acceptance rate for "Level 1" increased from 45% (green timber) to 85% (treated timber) in the most successful sample. LVMT-drying is a practical drying method for timber from large-diameter logs because it is effective in reducing residual stress and correcting warps while shortening the treatment period and avoiding thermal degradation.

Abstrakt w wersji dostarczonej przez źródło. Pełny tekst może być ograniczony przez wydawcę.