Douglas fir

Pseudotsuga menziesii · Softwoods

Properties

PropertyValueBasis of measurementSource
Density (about 12 % moisture) 510 kg/m³ Air-dried, about 12 % moisture content, mass over volume at that moisture The Wood Database Compiled from a secondary source, not yet cross-checked against a standard · 2026-10-22
Basic specific gravity 0.45 Basic specific gravity: oven-dry mass divided by green volume The Wood Database Compiled from a secondary source, not yet cross-checked against a standard · 2026-10-22
Radial shrinkage 4.5 % Radial shrinkage from green to oven-dry, percent of green dimension The Wood Database Compiled from a secondary source, not yet cross-checked against a standard · 2026-10-22
Tangential shrinkage 7.3 % Tangential shrinkage from green to oven-dry, percent of green dimension The Wood Database Compiled from a secondary source, not yet cross-checked against a standard · 2026-10-22
Volumetric shrinkage 11.6 % Volumetric shrinkage from green to oven-dry, percent of green volume The Wood Database Compiled from a secondary source, not yet cross-checked against a standard · 2026-10-22

Typical averages. Density and shrinkage vary between trees, growth sites and parts of the stem.

Use this species

Companies working with this species (0)

Research publications mentioning this species

Calculate drying shrinkage with the tangential value

Calculate the weight of 1 m³ at this density

Compare species