Effects of thermal and chemical treatments on colourimetric characteristics of young African mahogany and eucalypts wood for sawn timber production
Joyce de Almeida Pinto, Juarez Benigno Paes, Graziela Baptista Vidaurre, Ulysses Rodrigues Vianna, Djeison César Batista, Ana Carla Bezerra de Lima, Daniela Minini, Rodolpho Stephan Santos Braga, João Gabriel Missiada da Silva
3 luglio 2026 · Southern Forests a Journal of Forest Science
This publication is not marked as Open Access. The full text may require access through the publisher.
Summary
No reviewed summary yet. Read the abstract below or open the original publication.
Abstract
This study aimed to evaluate the effect of boron treatment and thermal modification on the wood colour of African mahogany species (Khaya ivorensis, K. senegalensis and K. grandifoliola) and eucalyptus (Eucalyptus grandis × E. urophylla) intended for sawnwood production. For this purpose, four logs measuring 50 cm in length were sampled along the tree trunk of the selected species, and 3-cm-thick discs were collected at the base of each log, to evaluate the basic density and its variation along the stem. The logs were converted into samples of 2.3 cm × 10.0 cm × 47.0 cm (thickness × width × length), which underwent treatments consisting of the control (no treatment), chemical treatment (boric acid and borax) using a 4% solution in which the samples were immersed until reaching a minimum retention of 0.5%, expressed as boric acid equivalent, and thermal modification (180 and 200 °C), applied for 120 min at the maximum temperature. The basic wood density varied along the trunk of the trees, particularly in K. grandifoliola (0.450–0.410 g cm-3), with K. senegalensis (0.542 g cm-3) showing density values similar to those of E. grandis × E. urophylla (0.586 g cm-3). Colourimetric analysis revealed that the treatments (chemical and thermal) promoted few variations in the colours (ΔE*) of the tangential (T) and radial (R) faces of the wood, except for the treatment at 200 °C, which caused darkening of the wood (K. ivorensis (ΔE*T = 10.01 − ΔE*R = 18.03), K. senegalensis (ΔE*T = 15.70 − ΔE*R = 21.25), K. grandifoliola (ΔE*T = 7.99 − ΔE*R = 11.76), and eucalyptus (ΔE*T = 9.50 − ΔE*R = 9.82)). However, the heat treatments standardised the color of the heartwood and sapwood.
Abstract as supplied by the source. Full text may be restricted by the publisher.
Related publications
Predicting the mechanical properties of sawn timber: Basic non-destructive tools applicable to Norway spruce sawlogs
1 set 2026 · Rostislav Berezjuk, Matěj Šimek, Robert Mařı́k et al. · Central European Forestry Journal
Evaluation of Wood Processing in the Sawmilling Industry in Ekiti State, Nigeria
1 lug 2025 · Ademola Ayodeji Omoyeni, Timileyin Samuel Oguntuase · International Journal of Advances in Engineering and Management
Moisture-induced timber joining - Utilizing the hygroscopicity and shape-memory effect of wood resulting in dimensional change in a prefabricated wood-only, self-built, sawn timber system for affordable housing in Colombia
1 mar 2024 · Max Salzberger, Juan Sebastian Cruz Rojas, Gilbert Koskamp · Research Square
Stakeholder Perspectives on Aligning Sawmilling and Prefabrication for Greater Efficiency in Australia’s Timber Manufacturing Sector
22 dic 2025 · Harshani Dissanayake, Tharaka Gunawardena, Priyan Mendis · Sustainability